Mechanical Properties |
Hardness, Shore A |
35 to 90 |
Tensile Strength, MPa |
4 to 22 |
Elongation, % |
150 to 800 |
Tear Strength, kN/m |
15 to 50 |
Compression Set, 70 hr at 150℃, % |
15 to 100 |
Electrical Properties |
Dielectric Constant |
2.8 |
Power Factor, % |
0.25 |
Dielectric Strength, kV/mm |
26 |
Volume Resistivity, Ohm-cm |
1 X 10^16 |
Thermal Properties |
Brittleness Point ,℃ |
-55 to -66 |
Minimum for Continuous Service, ℃ |
-50 |
Maximum for Continuous Service, ℃ |
150 |
Maximum for intermittent Service, ℃ |
175 |
Maximum Theoretical Temperature to Break Hydrocarbon Bonds, ℃ |
204 |